Performance

Physical Parameter

Type Specific Gravity(g/cm3) PH Appearance Consumption
(g/t.Ce)
Capacity increased by
(t/h)
 

Strength Increased(MPa)
Remark
TH-1 1.18-1.25 9-11 Brown liquid 280-350 8-15 If keeping the mill capacity, 3 days strength will be increased by 2-4MPa and 28days strength will be increased simultaneously. And 5-8% more additives can be used under this condition. Suitable for all kinds of cement.
TH-3 1.10-1.25 9-11 Brown liquid 220-250 8-15 If keeping the mill capacity, 3 days strength will be increased by 2-4MPa and 28days strength will be increased simultaneously. And 4-6% more additives can be used under this condition. Suitable for the cement with pozzolana, slag or flyash
TH-4 1.20-1.28 9-11 Brown liquid 480-550 8-15 If keeping the mill capacity, 3 days strength will be increased by 3-5MPa and 28days strength will be increased simultaneously. And 5-8% more additives can be used under this condition. Suitable for all kinds of cement.
TH-5 1.18-1.28 9-11 Brown liquid 1000-1200 8-15 If keeping the mill capacity, 3 days strength will be increased by 3-5MPa and 28days strength will be increased simultaneously. And 6-10% more additives can be used under this condition. Suitable for the cement with slag
 